AH bitumen is a bitumen grade that is popular in the China market. They categorized based on penetration value @ 25°C. AH grades are as below:

AH-50 Specifications


Specification of Infinity Galaxy Bitumen AH-50
SPECIFICATIONUNITVALUE TEST METHOD
Penetration1/10 Millimetres (mm40-50ASTM D5
Softening PointDegree Celsius (°C)48-56ASTM D36
Density, 25°CKilogram per Cubic Meter (kg/m³)1.000/1.060ASTM D71/D3289
Ductility, 25°CCentimetres per Second (cm/s)100 minASTM D113
Loss On HeatingWeight Percentage (WT%)0.2 MaxASTM D6
Drop-in Penetration After HeatingPercentage (%)20 maxASTM D6/D5
Flash Point (Cleveland Open Cup)Degree Celsius (°C)250 minASTM D92
Solubility in TrichloroethyleneWeight Percentage (WT%)99.5 minASTM D4
Spot TestNegative (−) or Positive (+)NegativeAASHOT 102 *
Bitumen ContentPercentage 99.9 minASTM D4


AH-70 Specifications


Specification of Infinity Galaxy Bitumen AH-70
SPECIFICATIONUNITVALUE TEST METHOD
Penetration 25°C1/10 Millimeters (mm)60-80ASTM D5
Softening PointDegree Celsius (°C)Min 42ASTM D36
Density, 15°CKilogram per Cubic Meter (kg/m³)1.000/1.060ASTM D70
Ductility, 15°C, 5CM/MINCentimetersMin 100ASTM D113
Ductility, 10°C, 5CM/MINCentimetersMin 20ASTM D113
Flash Point Degree Celsius (°C)Min 260ASTM D92
Dynamic Viscosity 60°CPoisesMin 130ASTM D2171
Solubility in TrichloroethyleneWeight Percentage (WT%)Min 99.5ASTM D 2042
Penetration Index-1.5/1.0
AFTER TFOT AT 163 ˚C ASTM D1754
LOSS Of WEIGHT-0.8/0.8ASTMD1754
RETAINED PENETRATION RATIO %Percentage(%)Min 61ASTM D5
Ductility, 25°C, 5CM/MINCentimetersMin 6ASTM D113


AH-90 Specification


Specification of Infinity Galaxy Bitumen AH-90
SPECIFICATIONUNITVALUE TEST METHOD
Penetration1/10 Millimetres (mm80-100ASTM D5
Softening PointDegree Celsius (°C)42-52ASTM D36
Density, 25°CKilogram per Cubic Meter (kg/m³)1.000/1.060ASTM D71/D3289
Ductility, 25°CCentimetres per Second (cm/s)100 minASTM D113
Loss On HeatingWeight Percentage (WT%)0.5 MaxASTM D6
Drop-in Penetration After HeatingPercentage (%)20 maxASTM D6/D5
Flash Point (Cleveland Open Cup)Degree Celsius (°C)225 minASTM D92
Solubility in TrichloroethyleneWeight Percentage (WT%)99 minASTM D4
Loss of WeightPercentage (%)0.8 maxASTM D1754
Retained Penetration After Thin FilmPercentage (%)50 minASTM D5
Ductility 25°C After Thin Film OvenCentimetres per Second (cm/s)100 minASTM D113
Ductility 15°C After Thin Film OvenCentimetres per Second (cm/s)100 minASTM D113
TemperatureDegree Celsius (°C)Max 90-110 above the Soft
Bitumen ContentPercentage (%)99.9 minASTM D4


AH-110 Specifications


Specification of Infinity Galaxy Bitumen AH-110
SPECIFICATIONUNITVALUE TEST METHOD
Penetration1/10 Millimetres (mm80-110ASTM D5
Softening PointDegree Celsius (°C)45-52ASTM D36
Density, 25°CKilogram per Cubic Meter (kg/m³)1.000/1.060ASTM D71/D3289
Ductility, 25°CCentimetres per Second (cm/s)100 minASTM D113
Loss On HeatingWeight Percentage (WT%)0.5 MaxASTM D6
Drop-in Penetration After HeatingPercentage (%)20 maxASTM D6/D5
Flash Point (Cleveland Open Cup)Degree Celsius (°C)225 minASTM D92
Solubility in TrichloroethyleneWeight Percentage (WT%)99 minASTM D4
Loss of WeightPercentage (%)0.8 maxASTM D1754
Retained Penetration After Thin FilmPercentage (%)50 minASTM D5
Ductility 25°C After Thin Film OvenCentimetres per Second (cm/s)100 minASTM D113
Ductility 15°C After Thin Film OvenCentimetres per Second (cm/s)100 minASTM D113
TemperatureDegree Celsius (°C)Max 90-110 above the Soft
Bitumen ContentPercentage (%)99.9 minASTM D4


AH-130 Specifications


Specification of Infinity Galaxy Bitumen AH-130
SPECIFICATIONUNITVALUE TEST METHOD
Penetration1/10 Millimetres (mm80-130ASTM D5
Softening PointDegree Celsius (°C)42-52ASTM D36
Density, 25°CKilogram per Cubic Meter (kg/m³)1.000/1.060ASTM D71/D3289
Ductility, 25°CCentimetres per Second (cm/s)100 minASTM D113
Loss On HeatingWeight Percentage (WT%)0.5 MaxASTM D6
Drop-in Penetration After HeatingPercentage (%)20 maxASTM D6/D5
Flash Point (Cleveland Open Cup)Degree Celsius (°C)225 minASTM D92
Solubility in TrichloroethyleneWeight Percentage (WT%)99 minASTM D4
Loss of WeightPercentage (%)0.8 maxASTM D1754
Retained Penetration After Thin FilmPercentage (%)50 minASTM D5
Ductility 25°C After Thin Film OvenCentimetres per Second (cm/s)100 minASTM D113
Ductility 15°C After Thin Film OvenCentimetres per Second (cm/s)100 minASTM D113
TemperatureDegree Celsius (°C)Max 90-110 above the Soft
Bitumen ContentPercentage (%)99.9 minASTM D4


Check out our article about bitumen tests that determine the quality of bitumen

Leave a Reply